Flotation Machine can be used to separate non-ferrous metal, ferrous metal, noble metal, non-metallic mine, chemical material. It can be used in roughing, scavenging, selection or reverse flotation. In the flotation process, after being mixed with drug, some qualified mineral attaches on bubble, floats on the surface of slurry and is scraped out, other mineral still stays in the slurry, so the separating purpose is finished.
Working Principle:
The impeller is rotated by V-belt of motor and produces negative pressure by centrifugal function. Enough air is sucked to mix slurry, and slurry mixes drug at the same time. Mineral sticks on bubble completely and floats on the surface of slurry to form mineralized bubble. Useful bubble is scraped out by adjusting flashboard height and controlling liquid surface.
Features:
1. Large inhaling capacity and low consumption.
2. Complete flotation circuit with inhaling air and slurry, no auxiliares are needed.
3. Process is easy to be changed.
4. Reasonable circulation of slurry decreases coarse sand sedimentation.
5. Automatic controlling device makes adjustment more convenient.
XJK series
| Model | XJK-0.13(1A) | XJK-0.23(2A) | XJK-0.35(3A) | XJK-0.62(4A) | XJK-1.1(5A) | XJK-2.8(6A) | |
| Volume (m3) | 0.13 | 0.23 | 0.35 | 0.62 | 1.1 | 2.8 | |
| Impeller Diameter (mm) | 200 | 250 | 300 | 350 | 500 | 600 | |
| Capacity (m3/min) | 0.05-0.16 | 0.12-0.28 | 0.18-0.4 | 0.3-0.9 | 0.6-1.6 | 1.5-3.5 | |
| Impeller speed (r/min) | 600 | 500 | 470 | 400 | 330 | 280 | |
| Scraper speed (r/min) | 17.5 | 17.5 | 17.5 | 26 | 26 | 26 | |
| Impeller motor | Model | Y100L1-4 | Y90L-4 | Y90L-4 | Y100L2-6 | Y132M2-6 | Y160L-6 |
| Power (KW) | 2.2 | 1.5 | 1.5 | 3 | 5.5 | 11 | |
| Scraper motor | Model | Y80M1-4 | Y80M1-4 | Y80M2-4 | Y80M2-4 | Y90S-4 | Y90S-4 |
| Power (KW) | 0.55 | 0.55 | 0.75 | 0.75 | 1.1 | 1.1 | |
Any change of technical parameters, there is no further notice.
SF series
| Model | SF0.37 | SF0.7 | SF1.2 | SF2.8 | SF4 | |
| Volume (m3) | 0.37 | 0.7 | 1.2 | 2.8 | 4 | |
| Impeller Diameter (mm) | 300 | 350 | 450 | 550 | 650 | |
| Capacity (m3/min) | 0.2-0.4 | 0.3-0.9 | 0.6-1.2 | 1.5-3.5 | 0.5-4 | |
| Impeller speed (r/min) | 352 | 400 | 312 | 268 | 238 | |
| Impeller motor | Model | Y90L-4 | Y100L2-4 | Y132M2-6 | Y160L-6 | Y180L-6 |
| Power (KW) | 1.5 | 3 | 5.5 | 11 | 15 | |
| Scraper motor | Model | Y90S-4 | Y90S-4 | Y90S-4 | Y90S-4 | Y90S-4 |
| Power (KW) |
1.1 |
1.1 |
1.1 |
1.1 |
1.5 | |
Any change of technical parameters, there is no further notice.

Welcome to Zoneding Machine, if you have any questions,please consult:+86-371-60305291 or +86-371-60305292, you can also leave your contact information,we will promptly contact with you.
![]() |
![]() |
![]() |
![]() |
We Got ISO 9001:2008 / CE / Bureau Veritas / SGS certificated. |