Application: Iron Ore,Tin,Chromium,Manganese,Niobium and tantalum,Rare earth,Industrial minerals,Heavy mineral sands,Garnet,Phosphate,Heavy media separation,Recycling.

Introduction: Magnetic separation separates the minerals according to magnetic intensity differences in Non-uniform magnetic field. the following are the main application of magnetic separation.
The separation of ferrous minerals: magnetic separation is the main processing way of iron ore, after the iron ore being processed, the ore grade will be improved,and the content of detrimental impurity will be reduced, which has a good effect on metallurgy smelting.
The separation of nonferrous and rare minerals: many nonferrous and rare minerals have different magnetic intensity, only gravity separation or only flotation separation can not have the good beneficiation effect, the combination of magnetic separation and gravity, flotation separation can have a good grade minerals.
The recovering of gravity separation medium, the magnetite and the ferrosilicon is the medium during the gravity separation.
Removing iron impurities from non-metallic mineral raw materials, iron removing can protect crushers and other equipment,the iron removing is very commen during nonmetallic mineral processing. Kyanite, quartz, red tourmaline, feldspar, nepheline diorite applies dry magnetic separation for a lone time.
The recovery of steel slag from the metallurgy smelting and pollutant removing from sewage: the great amount of steel slag in the metallurgy smelting. The steel slag can be recovered by dry grinding and dry magnetic separation.
Application of high gradient magnetic separation or deal with the sewage to remove the impurities.
100t/d for iron minerals :
| Item | Model | Quantity(set) | Power(KW) | Remarks |
| Jaw crusher | PE400×600 | 1 | 30 | |
| Jaw crusher | PEX250×1000 | 1 | 37 | |
| Feeder | Ф600×600 or GZ 1 | 1 | 2.2 | |
| Ball mill | Ф1500×3500 | 1 | 75 | |
| Classifier | Ф750 | 1 | 5.5 | Replacable |
| High frequency screen | GPS6 | 2 | 1.5×2 | |
| Magnetic separator | CTB918 | 1 | 4 | |
| Magnetic separator | CTB718 | 1 | 3 |
Any change of technical parameters, there is no further notice.
500t/d for iron minerals :
| Item | Model | Quantity(set) | Power(KW) | Remarks |
| Jaw crusher | PE500×750 | 1 | 55 | |
| Jaw crusher | PEX250×1000 | 1 | 37 | |
| Pendulum feeder | Ф600×600 | 1 | 2.2 | |
| Ball mil | Ф2100×4000 | 1 | 245 | |
| Classifier | Ф2000 | 1 | 7.5 | Replacable |
| High frequency screen | GPS6 | 2 | 1.5×2 | |
| Magnetic separator | CTB1021 | 2 | 5.5 |
Any change of technical parameters, there is no further notice.
1000t/d for iron minerals :
| Item | Model | Quantity(set) | Power(KW) | Remarks |
| Jaw crusher | PE600×900 | 1 | 75 | |
| Fine jaw crusher | PEX250×1000 | 2 | 45 | |
| Pendulum feeder | Ф800×800 | 1 | 3 | |
| Ball mil | Ф2700×3600 | 1 | 400 | |
| Classifier | Ф2000 | 1 | 15 | Replacable |
| High frequency screen | GPS8.1 | 2 | 2.2×2 | |
| Magnetic separator | CTB1224 | 2 | 7.5 |
Any change of technical parameters, there is no further notice.

Welcome to Zoneding Machine, if you have any questions,please consult:+86-371-60305291 or +86-371-60305292, you can also leave your contact information,we will promptly contact with you.
![]() |
![]() |
![]() |
![]() |
We Got ISO 9001:2008 / CE / Bureau Veritas / SGS certificated. |