Fine Crusher has many advantages, like reliable performance, easy structure, convenient maintenance, big capacity, long life hammer. It is widely used in granite, basalt, limestone, river gravel, cement clinker, quartz, iron ore, bauxite, etc. It is also used in road, railway, water conservancy, airport, construction, cement, refractories, metallurgy, etc.
Working principle:
When the Fine Crusher is working, materials are crushed primarily in the first crushing chamber by the high speed moving rotor against the hammer, and then enter the secondary chamber for fine crushing, at last, the final materials are discharged.
| Model | Inlet size (mm) | Feed Size (mm) | Out-put size (mm) | Capacity(t/h) | Power (kw) |
| PXJ0808 | 550×330 | <150 | 0-20 | 55-65 | 55 |
| PXJ1010 | 1000×350 | <150 | 0-20 | 65-75 | 75 |
| PXJ1212 | 1200×450 | <180 | 0-20 | 90-100 | 132 |
| PXJ1414 | 1500×500 | <180 | 0-20 | 100-150 | 260 |
| PXJ1616 | 1600×550 | <180 | 0-20 | 190-250 | 250 |
| PXJ1818 | 1800×800 | <180 | 0-20 | 280-310 | 315 |
Any change of technical parameters, there is no further notice.

Welcome to Zoneding Machine, if you have any questions,please consult:+86-371-60305291 or +86-371-60305292, you can also leave your contact information,we will promptly contact with you.
![]() |
![]() |
![]() |
![]() |