This crushing plant is used to crush stone with less than 1100mm, such as hard limestone, granite, basalt, pebble. Product with various sizes can be made according to customers’ special request in hydroelectric station, building materials, highway, railway, urban construction, etc. Impact crusher can be replaced by cone crusher according to customers’ request or hardness of stone.

| No. | Equipment | Model | Motor (KW) | Number |
| Hopper | LC3000X4000 | 1 | ||
| I | Vribrating Feeder | GZD1300x6000 | 15 | 1 |
| II | Jaw Crusher | PE1200x1500 | 180 | 1 |
| III | Impact Crusher | PF1320 | 315 | 2 |
| Ⅳ | Vribrating Screen | 3YK2460 | 37 | 2 |
| Belt | ||||
| No. | Name | Length (m) | Motor (KW) | Number |
| B1 | B500 | 20 | 11 | 1 |
| B2 | B1500 | 26 | 30 | 1 |
| B3 | B1500 | 28 | 30 | 2 |
| B4 | B1200 | 30 | 22 | 1 |
| B5 | B800 | 20 | 11 | 6 |

Welcome to Zoneding Machine, if you have any questions,please consult:+86-371-60305291 or +86-371-60305292, you can also leave your contact information,we will promptly contact with you.
![]() |
![]() |
![]() |
![]() |
We Got ISO 9001:2008 / CE / Bureau Veritas / SGS certificated. |