Product List

Spiral Chute

  • 点击浏览Next

    Structure:
    Fiber Glass Spiral Chute is made up of feeder, feed chute, spiral flute, bracket, intercepting slot, gathering slot.
    Features:
    Spiral Chute has such features as: simple structure, easily being-operated, reliable operation, easy maintenance,
    smaller area, high capacity.
    Application:
    It is used to process iron, stannum, tungsten, tantalum, niobium, gold ore, colliery, monazite, rutile and Zircon of the
    size between 0.3 and 0.02mm, and the other metals nonmetal minerals with enough proportion deviation.Сепаратор
    спиральный предназначен для обогащения угольных шламов крупностью 0,1-3 мм.
    Main Technical Parameter:

    Model

    Helix No.

    Cycle

    Feed Size (mm)

    Feed Density ( %)

    Production (t/h)

    Area(m2)

    Height(m)

    DL2000

    2-4

    3-5

    0.04-4

    20-45

    15-45

    5.7

    6.6

    LL1200

    2-4

    4-5

    0.03-0.3

    25-50

    4-6

    2

    5.23

    LL900

    2-3

    4-5

    0.03-0.3

    25-50

    2-3

    1.2

    3.2

    LL600

    1-2

    4-5

    0.02-0.2

    25-50

    0.8-1.2

    0.5

    2.6

    LL400

    1-2

    4-5

    0.02-0.2

    25-50

    0.5-0.2

    0.25

    1.5

    Technical parameter fluctuation doesn't go another notice