Product List

DC-type magnetic separator

  • 点击浏览Next

    Applications

    STC type magnetic separator(dry-type magnetic separator) is mainly applicable for the coarse granule magnetic
    mineral like beach placer and river sand. It is also could be used at the primary separation of the magnetic mineral.
    The grade of the coarse ore could be up 60%.
    Working Principle

    The material inpours from the input port and the magnetic material in it absorbs on the surface of the tank under the
    action of the magnetic field. With the rotating of the tank when the magnetic material disengages from the magnetic
    field it falls into the chute under the action of the gravitation. The nonmagnetic material was thrown into the tailings
    chute under the action of the inertia and gravitation with the rotating of the tank. Then the magnetic material and
    nonmagnetic material are separated, the separation work ends.
    Characteristics:
    1. Simple installation and adjustment, easy to cooperate.
    2. The use of permanent magnetism reduces the cost of using and maintenance.
    3. Wet and dry dual-use, wide range of application.
    4. Easy to move and connect with other equipments.

    main technical parameter:

    model

    tank size(mm)

    magnetic field strength (GS)

    power(KW)

      Rotational (M/S)

    weight (KG)

    STC-618

    600×1800

    2500

    3.0

    87

    1320

    STC-718

    700×1800

    2500

    4.0

    87

    1500

    STC-7520

    750×2000

    2500

    4.0

    81

    1870

    STC-7522

    750×2200

    2500

    5.5

    81

    2050

    STC-7524

    750×2400

    2500

    7.5

    81

    2420

    STC-8526

    850×2600

    3000

    7.5

    76

    2750

    STC-8528

    850×2800

    3000

    11

    76

    3050

    STC-8530

    850×3000

    3000

    11

    76

    3300

    Technical parameter fluctuation doesn't go another notice