Product List

Jaw Crusher

  •  点击浏览Next

     点击浏览Next

    Zoneding Jaw Crusher series are based on years’ experience and technology development. The continuous
    improvement and refinement has made them the preferred jaw crusher for professionals and our customers. They can
    meet most crushing requirements in primary and secondary crushing, and the largest compression resistance of the
    material is 320MPa. This series are widely used in stone mining, metallurgical, construction, smelting, hydraulic and
    chemical industries, etc.

    Working principle of Jaw Crusher:
    The motor transmits power through belt, drives the moving jaw to do periodic motion towards the fixed jaw by the
    eccentric shaft. The angle between toggle plate and moving jaw plate increases when moving jaw moves. So the moving jaw moves towards the fixed jaw. The stuff will be crushed in this process. The angle between toggle plate and moving
    jaw decreases when moving jaw moves down, the moving jaw moves leaves fixed jaw by pulling rod and spring, the
    final crushed stuff will be discharged from the outlet.

    Characteristics of Jaw Crusher:
    -High crushing ratio
    -Even product granularity
    -Simple structure
    -Wide ranges of choices
    -Reliable working condition
    -Convenient maintenance

    main technical parameter:

    Model

    Feeding inlet size (mm)

    Max feeding size(mm)

    Discharge size(mm)

    Capacity(t/h)

    Motor power(kw)

    Вес (t)

    PE-150

    150×250

    125

    15-45

    1.2-3.5

    5.5

    0.6

    PE-250

    250×400

    210

    20-60

    5-22

    15

    2.8

    PE-400

    400×600

    340

    40-80

    18-60

    37

    7

    PE-500

    500×750

    425

    50-100

    43-102

    55

    10.6

    PE-600

    600×900

    500

    65-160

    51-180

    75

    19.2

    PE-750

    750×1060

    630

    80-180

    80-195

    110

    29

    PE-900

    900×1200

    780

    95-180

    140-270

    132

    51

    PE-1000

    1000×1200

    850

    195-280

    190-310

    132

    55

    PE-1200

    1200×1500

    1020

    150-300

    260-510

    160

    100.9

    PEX-150

    150×750

    120

    18-40

    8.5-28

    15

    3.8

    PEX-250 250×750 210 25-60 15-35 30 5.1
    PEX-250 250×1000 210 25-60 20-65 37 7
    PEX-250 250×1200 210 25-60 25-75 45 8.5
    PEX-300 300×1300 250 20-90 30-105 75 11.9

     

    Technical parameter fluctuation doesn't go another notice
Combination Crusher   Roll Crusher