Product List

Sand Making Machine

  •  点击浏览Next

     点击浏览Next

    Zhongding ZDP vertical shaft impact crusher (namely, sand making machine) is the specialized machine with
    international advanced level. Technology and modern processing make it a leading role in this industry. It is widely
    used for artificial sand, in metal and non-metal ores, cement, refractory material, bauxite, silicon carbide, glass
    material, building material. The finished sand has even particle size, high compressive strength, and high-purity.

    The stones fall from the top of the machine, and then it is divided into two parts by material-dividing plate. One enters
    into high-speed rotating impellor through the center of material-dividing plate. The other falls down from outside of
    material-dividing plate. Under the action of the high speed centrifugal force, the stones crushed the others distributed
    around the impeller in the form of umbrella. After the stones impact each other, the eddying motion is formed between
    the impeller and main case to bring about many times’ mutual impacting, rubbing, and crushing till the granularity
    required is achieved.

    Features:

    -The machine is a new-type one, which is used widely to substitute Cone Crusher, Ball Mill and Rod Mill
    -New and unique construction and stable operation
    -Energy-saving, higher capacity, higher crushing ratio
    -Low noise, less dust pollution
    -Cubical product and great sand pile density
    -The stones can product the base of machine during the production
    -Some wearing parts are made of super hard and wear resistant materials.
    They have the small bulk and light weight, so that they can be changed easily.
    -Small volume, simple operation, and easy installation and maintenance.

    Main Technical Parameter:

    Model

    Max Feeding Size (mm)

    Rotating plate diameter (mm)

    Rotating speed
    (r/min)

    Power
    (kw)

    Capacity
    (t/h)

    Weight (t)

    ZDP550

    40

    550

    2000-3000

    37-55

    25-55

    3.85-4.6

    ZDP750

    45

    750

    1500-2600

    75-110

    65-120

    6.85-7.6

    ZDP860

    50

    860

    1200-2000

    110-150

    110-180

    10-11.6

    ZDP1050

    60

    1050

    1000-1750

    132-220

    190-270

    16-17

    ZDP1250

    70

    1250

    950-1350

    264-400

    280-380

    18-19

    Technical parameter fluctuation doesn't go another notice