Product List

Mill Equipment

  • 点击浏览Next    点击浏览Next

    Our company has the annual output of 44,000 tons, 88,000 tons, 100,000 tons, 200,000 tons and 300,000 tons complete
    cement production line. We can provide on-site design, materials experimental, equipment installation and debugging, and
    the turnkey project of complete production line.
    Model PMG series high efficient ball mill have been designed with the merits of open circuit grinding system and important
    renovations on traditional ball mills. Besides they have all the good advantages of open circult mills,production capacity
    has been raised substantially, product becomes super fine and blains have been increased.It has provided a new type of
    grinding equipment for producing high strength grade cement with high output and super finess.
    Model PMG ball mill has adopted special intergrate diaphragm and discharge grate to adjust material levels of every
    chamber so as to increase air ventilation and improve conditions inside mill; meanwhite it has also used new type of lining
    plate ,regulated mill rotation speed, optimized design of bearings so as to increase its operational stability,use life and
    grinding efficiency.
    After being put into practice, it is proved that its output has been increased about 20% and unit product power consumption has been reduced 10%-12% down under the conditions that other parameters have not been changed by comparison to
    other same sized ball mill. White being operated in open circuit, specific surface of cement could be reached up to
    320cm2/kg Performance of it is up to national advanced standard .It has been awarded as well-known Brand Product of
    China Buliding Material Machinery Industry, "Well know Brand Products"," Appointed Manufacture of National Building
    Material Machinery Industry" and etc.
    main technical parameter:

    cement mill

    Specification (D×L) Rotary speed
    (r/min)
    Feed size(mm) capacity (t/h) Loading capacity of grinding medium
    (t)
    Main motor Main reducer weight
    (t)
    Model Power (kw) Rotary speed (r.p.m) Model Speed ratio
    φ2.2×11 20.91 ≤25 15~17 50 TR1512-8 570 740 Zd80 5.6 92
    φ2.4×8 20.91 ≤25 14~18 39.5~42 TRQ1512-8 570 740 Zd80-9 5 76.4
    φ2.4×9 20.91 ≤25 closed 23~25 50 TR1512-8 570 740 Zd80-9 5 91
    φ2.4×10 20.91 ≤25 16~22 50 TR1512-8 570 740 Zd80-9 5 111
    φ2.4×11 21 ≤25 open 19~24
    closed 22~28
    6265 YR710-8/1180 710 740 JDX630 5.6 125
    φ2.4×12 21 ≤25 open18~20
    closed21~23
    6365 YR800-8/1180 800 740 MBY710 6.3 127
    φ2.4×13 21 ≤25 open21~22
    closed24~26
    6668 YR800-8/1180 800 740 MBY710 6.3 131
    φ2.6×10 20.6 ≤25 21~24 64 YR800-8/1180 800 740 JDX710 6.3 140
    φ2.6×13 20.6 ≤25 28~31 81 YR1000-8/1180 1000 740 JDX800 6.3 158
    φ3.0×9 19.13 ≤25 40~45 85 YR1000-8/1180 1000 740 MBY800 7.1 148
    φ3×11 18.92 ≤25 44~47 95 YR1250-8/1430 1250 740 JDX900 7.1 177
    φ3×12 18.92 ≤25 48~52 103 YR1250-8/1430 1250 740 JDX900 7.1 182
    φ3×13 18.92 ≤25 39~45 116max YR1400-8/1430 1400 740 JDX900 7.1 200.7
    φ3.2×11 18.3 ≤25 45~48 112max YR1600-8/1430 1400 740 JDX900 7.15 213.6
    φ3.2×13 18.7 ≤25 50~55 133max YR1600-8/1430 1600 740 JDX1000 7.15 237
    φ3.4×11 18 ≤25 45~55 120max YR1600-8/1430 1600 740 JDX1000
    230
    φ3.5×13 17 ≤25 60~65 156max YR2000-8/1730 2000 740 TS130-A-F1
    257.6
    φ3.8×13 (main bearing type) 17 ≤25 65~70 190 YR2500-8/1730 2500 740 JS130-C-F1
    316
    φ3.8×13 (side sliding shoe type) 17 ≤25 65~70 185 YR2500-8/1730 2500 740 DMG22/2500
    313
    φ4×13 16.3 ≤25 78~80 191 YRKK900-80 2800 745 JS140-A
    348
    φ4.2×11 (main bearing type) 15.8 ≤25 100~110 182~190 YR2800-8/17830 2800 740 JS140-A-F1D
    350
    φ4.2×13 (main bearing type) 15.2 ≤25 110~120 230 YRKK1000-8 3350 740 MFY355-A
    375
    φ4.2×13 (main bearing type) 15.2 ≤25 120~130 245 YRKK1000-8 3350 740 MFY355-A
    390
    φ4.2×13 (center sliding shoe type) 15.2 ≤25 110~120 230 YRKK1000-8 3350 740 MFY355-A
    380
    φ4.6×14 15 ≤25 100~115 285 YR1000-8 4200 740 J3160-C
    485

    Drying Raw Mill

    Specification (D×L) Rotary speed
    (r/min)
    Feed size (mm) capacity (t/h) Loading capacity of grinding medium (t) Main motor Main reducer weight
    (t)
    Model power(kw) Rotary speed(r.p.m) model Speed ratio
    φ3×(8.5+5) 18.9 ≤25 55~53 76~80 YR1000-8/1180 1000 740 JDX800 6.3 160
    φ3.2×(7+1.8) (cantilever drying) 18.25 ≤25 50~53 59 YR630-8 1000 740 JDX800 6.3 153
    φ3.5×10 (cantilever drying) 17.3 ≤25 75~80 87 YR1250-8/430 1250 740 JS110-A-F1 214
    φ3.6×(7.5+1.5) 17.3 ≤25 90~95 98 YRkk710-8 1400 740 JDX900 7.1 220
    φ3.8×1.2 16.6 ≤25 133 100~110 YR800-8 2000 740 JS130-A 295
    φ4.6×(9.5+3.5) 15 ≤25 185 175~180 YRkk1000-8 3550 740 MFY355A 415

    Wet process raw mill

    Specification (D×L) Rotary speed
    (r/min)
    Feed size (mm) capacit y(t/h) Loading capacity of grinding medium
    (t)
    motpr Main reducer weight
    (t)
    type power(kw) rotary speed(r.p.m) type Speed ratio
    φ2.2×7 21.4 ≤3 20~25 31 YR148-8 380 740 ZD70-9 5 49
    φ2.2×13 21.6 ≤25 33~37 58~60 YR630-8/1180 630 740 MBY630 5.6 53.4
    φ2.4×13 21 ≤25 45~50 65~70 YR800-8/1180 800 740 JDX710 5.6 131
    φ2.6×13 20 ≤25 45~46 80t(max) YR1000-8/1180 1000 740 TDX800 6.3 153
    φ6.2×6.4 18.5 ≤25 32~41 86~90.5 TDMK1000-36 1000 740 134

    Dry Process Raw mill

    Specification (D×L) Rotary speed
    (r/min)
    Feed size(mm) capacity (t/h) Loading capacity of grinding medium
    (t)
    motor Main reducer weight
    (t)
    model power(kw) Rotary spee d(r.p.m) model Speed ratio
    φ2.4×8 20.91 ≤25 25~28 39~42 JRQ1512-8 570 740 ZD80-9 5 76.4
    φ2.4×10 20 ≤25
    open27~30
    closed38~40
    50 YR710-8/1180 710 740 JDX630 5.6 111
    φ2.4×11 21 ≤25
    open41~42
    closed46~48
    62~65 YR800-8/1180 800 740 MBY710 6.3 125
    φ2.4×12 21 ≤25
    open40~42
    closed45~48
    63~65 YR800-8/1180 800 740 MBY710 6.3 127
    φ2.4×13 21.5 ≤25 48~51 68~72 YR800-8/1180 800 740 MBY710 6.3 131
    φ2.6×8 20 ≤25 30~35 54 YR630-8/1180 630 740 JDX630 5.6 135
    φ2.6×10 20.91 ≤25 45~46 80 YR1000-8/1180 1000 740 JDX710 6.3 136
    φ3×9 19.13 ≤25 50~55 76~80 YR1000-8/1180 1000 740 JDX800 6.3 145
    φ3.2×7 18.25 ≤25 50~52 58 YR1000-8/1180 1000 740 MBY800 6.3 140
    φ3.2×9 18.3 ≤25 60~70 90 YR1250-8/1430 1250 740 JDX900 7.1 175
    φ4.6×10+3.5 15 ≤25 195 190 3550 740 JS150-B-F 476

    Wind swept mill

    Specification (D×L) Rotary speed
    (r/min)
    Feed size (mm) (t/h) capacity Loading capacity of grinding medium
    (t)
    Motor Main reducer Weight
    (t)
    Model Power(kw) Rotary speed(r.p.m) Type Speed ratio
    φ2.2×4.4 22.4 ≤25 8~9t/h 18t YRKK4501-6 250 986 ZD60-11 6.3 36.7
    φ2.2×5.8 22.4 ≤25 5.5~7 23.5~25 Y4005-8 280 750 ZD70-10 5.6 45
    φ2.4×4.75 21.2 ≤25 14 22~24 YR4501-8 315 740 ZD60-8 4.5 49
    φ2.4×4+2 20.2 ≤25 10~11 19 YRKK450-8 250 740 ZDY355 4.5 60
    φ2.4×4.5+2 20.2 ≤25 10~12 20.8 YRKK500-8 280 740 JDX45 4.5 68
    φ2.6×(5.25+2.25) 19.7 ≤25 9~10 28 YRKK500-8 400 740 ZDY450 4.5 87.4
    φ2.8×(5+3) 18.7 ≤25 13~13.5 32 Y5001-8 500 740 JDX560 4.5 102
    φ2.9×4.7 19.1 ≤25 14~19 34.4 YR560-8 500 743 MBY560 5.6 79
    Technical parameter fluctuation doesn't go another notice