    Mica Ore Processing

           Mica is belongs to Aluminum silicate minerals. It has continuous layer silica tetrahedron structure. In industrial, the white mica is the most common ore, gold mica is following.  It is mainly used as electric equipment and insulating materials in electric equipment. it is also used in mechanical parts using in manufacturing steam boiler, smelting furnace.  In addition, it is widely used in paint, rubber, plastic package and building materials.

     

            The density of mica is 2.7~3.1t/m3, hardness is 2.0-2.5, it is flake structure.
     

            The main originals of mica are India, Russia, Brazil, America, etc. our country is also rich in mica, the main originals are Sichuang, Xinjiang, Qinghai, etc. 
     

            The main methods of beneficiating Mica are follows:
            1. Manual method: on the ore pile or breast, pick up the mica which is monomer separated; if the mica and gangue are adenosines, we can break them by hand, and then pick up the mica.
            2. Forming beneficiation: the Mica and gangue are separated by dual-vibrating screen according to the different forms. The upper layer is using bar screen and lower layer is using square screen, so the gangue and mica is separated. This method has features of little investment, simple production process, high efficiency and better beneficiation result. So this is the common method for mica beneficiation.
            3. Flotation: mica is separated from undressing ore through crushing and grinding, and we can get mica concentrate. Mica flotation can be finished in acidic or alkaline slurry. Broken mica can be finished beneficiation in flotation machine.
            4. Dry blowing: its process is crushing—screening—dry blowing. According to the different form and suspension speed in air, we can finish the dry blowing process through beneficiation equipments. This method is suitable to the dry areas.
           From the perspective of trend development, the demand of mica powder will be increased, because the mount of mica is decreased. so the mica flotation is the trend of beneficiating mica powder. 
            

            The topical case of mica beneficiation is Danba mica beneficiation in Sichuang Province, Lingshou mica beneficiation in Hebei, etc.

    Order Online

    If you have some questions about our products, please feel free to fill out the form below, and we will contact you within 24 hours. Rest assured that we won’t reveal your information to anyone.

    Your Name: *
    Email: *
    Country:
    Tel.:
    Product:
    Please enter detailed information in the form below, such as raw materials, capacity(t/h,t/d), materials feeding size(mm), finial products size(mm) or other requirements.
    Message: *
     
    ABOUT US
    About Zoneding
    Zoneding Certifications
    Zoneding FAQ
    Zoneding Cases
    Zongding Service
    PRODUCTS
    Crushing & Screening Equipment
    Beneficiation Equipment
    Mobile Crushing Plant
    Grinding Plant
    Drying Equipment
    SOLUTIONS
    Different Materials Crushing Line
    Different Capacities Crushing Line
    Minerals Beneficiation Plant
    CONNECT WITH US
    LinkedIn® Find, connect, and collaborate. ---- Join Us
    Twitter® Instant updates about what's going on. ---- Follow Us
    Facebook® Connect with old and new friends. ---- Let's Be Friends
    google+

    Copyright:2014 Zhengzhou Zhongding Heavy Duty Machine Manufacturing Co.,Ltd.