Brief Introduction:
Magnetic separator is used for wet magnetic separation, separating materials with granularity below 3mm, such as magnetite, hematite, limonite, pyrrhotite, ilmenite. It is also used for deironing of coal, nonmetallic ore, construction industry, etc.ZONEDING can provide magnetic separator of forward flow, semi counter flow and counter flow types as customers’ requirements. We can provide magnetic separators of forward flow, semi counter flow and counter flow types as customers’ requirements.
Features:
1. High magnetic intensity;
2. Low energy consumption;
3. Good beneficiating efficiency;
4. Simple structure and easy maintenance. Slurry enters chute through ore tank, and then gets into separating zone by waterpower. Minerals with strong magnetism is absorbed on the barrel’s surface under the force of magnetic field and get into the ore concentrate outlet along with the rotation of cylinder. After leaving the magnetic field, they flow into ore concentrate box by the action of gravity and flushing water. Gangue and ore with weak magnetism are discharged into a pipe in the opposite direction of cylinder rotation.
Model | Shell Diameter (mm) | Shell length (mm) | Feed size (mm) | Capacity (t/h) | Power(kw) | Weight (t) |
CTB612 | Φ600 | 1200 | 0-2 | 10-20 | 1.5 | 1.5 |
CTB618 | Φ600 | 1800 | 0-2 | 15-30 | 2.2 | 1.8 |
CTB718 | Φ750 | 1800 | 0-2 | 25-45 | 3.0 | 2.2 |
CTB918 | Φ900 | 1800 | 0-3 | 35-70 | 4.0 | 2.8 |
CTB1018 | Φ1050 | 1800 | 0-3 | 40-75 | 5.5 | 4.3 |
CTB1024 | Φ1050 | 2400 | 0-3 | 52-100 | 5.5 | 5.2 |
CTB1218 | Φ1200 | 1800 | 0-3 | 47-90 | 5.5 | 5.0 |
CTB1224 | Φ1200 | 2400 | 0-3 | 80-120 | 7.5 | 6.4 |
Any change of technical parameters, there is no further notice.
cobblestone
Limestone
Dolomite
Quartz
Weather fossil
Granite
Coal gangue
Iron ore