Spiral Classifier
  • 【Spiral Diameter】: 500-3000mm
  • 【Power】: 3-40kw
  • 【Processible Materials】: Natural sand, artificial sand, machine-made sand.
  • 【Application】: Clean mud and water or working with ball mill to control material size.
Features Pictures&Videos Specifications Applications Cases Related Products
Features

Brief Introduction:

Spiral Classifier is widely used to control material size from Ball Mill in the beneficiation process, separate mineral sand and fine mud in the gravity concentration, and clean mud and water in washing mineral process. This machine has features of simple structure, reliable and convenient operation, etc.

Features:

1.Simple structure, stable operation, safe and reliable;

2.The main screw frame electric lifting device of the standard configuration, making the equipment operation and replacement of spare parts more easy. 

3.Optimization design of the helical blade, making sure of spare parts to minimize loss.

Pictures&Videos

Spiral Classifier(图1) Spiral Classifier(图2)

Spiral Classifier(图3) Spiral Classifier(图4)

Specifications
ModelSpiral diameter (mm)Speed of Spira l(r/min)CapacitySlope (°)Powe r(KW)Weight (t)
Sand Return (t/h)Overflow (t/h)
FL-55008-15.5143-26113212-1831.9
FL-77504.5-10256-5646512-1832.7
FL-1010001.6-7.4473-10268512-185.54.1
FL-1212005-71170-160015512-185.57.5
FL-1515002.5-670-11523512-187.510.5
FL-1818002.5-6100-190

310

12-181117.1
FL-2020002.5-6160-23040012-181519.3
FL-2424003.64160-23058012-1818.526

Any change of technical parameters, there is no further notice.