  • 【Feed Size】: ≤25-≤100mm
  • 【Capacity】: 5-210t/h
  • 【Processible Materials】: Limestone, slag, coke, coal, salt, chalk, gypsum, alums, brick, tile, etc.
  • 【Application】: To crush medium and high hardness materials in the industries of cement, electricity, chemical engineering, metallurgy, construction materials and refractory matter.
Features Pictures&Videos Specifications Applications Cases Related Products
Features

Brief Introduction:

Roller crusher is mainly used for secondary and fine crushing to materials below middle hardness, such as coking coal, clinker mineral, limestone, metallic and nonmetallic ore. Roll crusher is available for ore dressing, chemical, cement, refractories, abrasive, building materials industries, finely crushing all kinds of ore and rock below the high, medium hardness,which can make the minimum grain size below 100 mesh,especially in the building materials industry to produce melon meters stone and green bean products etc, and have the more excellent effect than general stave machinery , in recent years, also widely used in crushing steel grit industries.

Features:

1.It's available for ore dressing, chemical, cement, refractories, abrasive, building materials industries;

2.Roll crusher has the more excellent effect than general stave machinery;

3.Finely crushing all kinds of ore and rock below the high, medium hardness,which can make the minimum grain size below 100 mesh;

4.Roller crusher is stable operation, easy maintenance, low cost, output size adjustable.

Pictures&Videos

Roller Crusher(图1) Roller Crusher(图2)

Roller Crusher(图3) Roller Crusher(图4)

Specifications
Model2PG400×2502PG610×4002PG600×7502PG900×9002PG900x1200
Diameter of roller (mm)400610600900900
Length of roller (mm)2504007509001200
Max. feeding size (mm)≤25≤40≤40≤50≤50
Discharging size (mm)2—82—252—252-302—30
Capacity (t/h)5—1013—4060—12570-15090-210
Roller number22222
Rotating speed (r/min)18075654141
Weight (t)1.84.56.51518
Overall Dimension (L×W×H) (mm)1215×834×8303600×1590×11703560x1910x10055665x2530x16465665x2830x1646
Power (KW)2×5.52×152×222×372×45

Any change of technical parameters, there is no further notice.