Brief Introduction:
This crusher is designed and optimized according to crushing technology at home and abroad, its performance has reached the advanced level, for crushing all kinds of hard ores, can be widely used in mining, metallurgy, refractory, cement , coal, glass, ceramics, and electric power industries. Compound crusher has big crushing ratio, the discharged size can be adjusted, not affected by the weariness of hammer board and the impact liner, Due to no screen bar setting, it can crush high moisture and mud materials, but not be clogged.
Compound crusher, is widely used in stone crushing line or sand production line. This series crusher is suitable for crushing limestone, clinker, coal and other minerals of building materials, mining, metallurgy, chemical industry. its compressive strength is not more than 140 Mpa, humidity less than 15%.
Features:
Our compound crusher has large crushing ratio, higher yield, with 1.4 times yield than other crushers. It has efficient crushing capacity for shale, glass, ceramics, river gravel, granite, basalt, iron ore, bluestone, metal ores and other hard materials, particularly widely used in the mechanism aggregates and metal ores. Its wearing parts employ multi-alloy wear-resistant materials with high hardness, high toughness, life expectancy increased by 2-3 times; the gap between hammer and impact plate is adjustable, to meet the crushing requirements of variety materials.
1.large crushing ratio, no screen bar, no clogging when crushing high moisture and mud materials.
2. Bearings horizontal arrangement, long life, can crush high temperature materials (such as cement clinker).
3. Adopt flexible adjustment mechanism, the non-crushing materials can be automatically discharged, will not damage the equipment.
4. The rotor block is unique structure; the rotor block will not wear. The back cavity is with screw rod or hydraulic opening mechanism; you can easily replace wearing parts. not opening the equipment.
Model | 800 | 1000 | 1250 | 1500 | 1750 | |
Rotater Diameter(mm) | 650 | 800 | 1000 | 1250 | 1560 | |
Cylinder Height(mm) | 800 | 850 | 850 | 1000 | 1410 | |
Rotating Speed(r/min) | 1350 | 970 | 740 | 650 | 600 | |
Input Size(mm) | 50 | 70 | 100 | 100 | 100 | |
Output Size (mm) | 0-5 | 0-5 | 0-5 | 0-5 | 0-5 | |
Capacity (t/h) | 5-15 | 10-30 | 20-60 | 30-80 | 40-100 | |
Motor | Power(kw) | 30 | 55 | 75 | 110 | 132 |
Rotating Speed | 1440 | 1440 | 750 | 750 | 750 | |
Overall Dimension(L×W×H)(mm) | 2200×860×1980 | 2700×1160×2000 | 2800×1400×2730 | 3100×1900×2300 | 3350×2100×2800 | |
Weight (t) | 2.3 | 4.5 | 9.73 | 18.1 | 26.61 |
cobblestone
Limestone
Dolomite
Quartz
Weather fossil
Granite
Coal gangue