Chromite Ore Processing
2019-08-09 10:57:13 小编

  Chromite is found in peridotite from the Earth's mantle. It also occurs in layered ultramafic intrusive rocks. In addition, it is found in metamorphic rocks such as some serpentinites. Ore deposits of chromite form as early magmatic differentiates. It is commonly associated with olivine, magnetite, serpentine, and corundum.

  Major components:

  (Fe, Mg)Cr2O4

  Mohs hardness:

  5.5

  Available machine:

  Jaw Crusher ,Ball Mill,Vibrating Screen

  Applications:

  Metallurgical,Refractory,Chemical

  Introduction of chrome ore beneficiation plant:

  Ore dressing means the production process in which the extracted ore goes through several procedures finally becomes the concentrate in accordance with the smelting requirements. Ore dressing flow mainly includes crushing by crusher, separating by vibrating screen, grinding by ball mill and classifying by classifier; the separation of minerals consists of weight, flotation, and electric separation, etc. Dehydration of minerals includes enrichment, filtration, drying, and other procedures. The equipment of mineral processing cover feeder, crusher, ball mill, classifier, vibrating screen, rocking bed, magnetic separator, mix tank, flotation machine and so on.

  Working principle of chrome ore beneficiation plant:

  The extracted ore should be crushed by jaw crusher initially. When it gets the reasonable fineness, it is transported into ball mill by elevating conveyer and feeder, and is milled by ball mill. The subtle milled ore gets the next procedure: classification. There is a theory that if the weights of solid particles are different, the sedimentations will be different, and the mixed ore can be classified by screw classifier. The classified ore gets into magnetic separator. Since the specific magnetization coefficients of ores are different, the magnetic substance of mixed ore is separated from others with magnetic and mechanical force. The mineral matter, which has been separated by magnetic separator initially, is transported into flotation machine by, and different medicines are added according to different characteristics of ore, so that the needed ore is separated from others. Since the separated ore are wet, they should be dewatered by thickner initially, and dried by drier. Finally, the dry minerals come into being.