Manganese Ore Processing
2019-08-09 10:59:42 小编

  Manganese ore is the ore materials containing manganese. It is widely used in steel industry, chemical industry, light industry, building materials industry, national defense industry, electronic industry, as well as agriculture industry.

  Manganese ore, mostly belonging to lean ore, must go through the dressing process;Most of the manganese ore stones are embedded in fine grain or subtle grain form and there are a number of high phosphate rock, high iron ore and symbiotic beneficial metal. For above two reasons, dressing process has great difficulty. At present, the commonly used manganese ore dressing methods are as follows:

  1.Ore washing and screening.

  2.Re-election.

  3.Strong magnetic separation.

  4.Re - magnetic.

  5.Magnetic-flotation.

  6.Pyrogenic process beneficiation.

  7.Chemical choosing method for manganese.

  Basic Process of ZONEDING ore beneficiation and upgrading plant

  The basic process for the line is primary crushing (Jaw Crusher), Secondary Crushing (Fine Crusher, Impact Crusher,Cone Crusher), Grinding (Ball Mill), Washing and Screening (spiral classifier, vibrating sieve) , Flotation(flotation machine),Separating (magnetic separation,shaking table, jig).