How Silver Is Mined: The Complete Ore to Ingot Process

Blog 35110

A key fact about how silver is mined is that it is rarely the primary target. Over 70% of the world’s silver is a by-product of mining lead, zinc, and copper. This occurs because silver is almost always found chemically bonded or mixed within other minerals. Therefore, the silver mining process is not about isolating silver directly. It is about executing a complex metallurgical operation to separate silver from other metals. This guide explains the complete silver processing sequence, from rock in the ground to a pure metal ingot.

silver mining

How Do You Find a Silver Deposit in the First Place?

Exploration does not typically target silver alone. Geologists look for its associated metals: lead, zinc, and copper. Because silver atoms are often located within the crystal structure of minerals like Galena (lead sulfide), geologists search for large sulfide systems. This exploration involves surface geological mapping and analyzing geochemical data from soil and rock samples. Promising targets are investigated with geophysical surveys that can detect dense sulfide bodies underground. Final confirmation comes from drilling. Core samples are extracted from the rock and sent to a laboratory for analysis. A deposit is considered economic only if the combined value of all recoverable metals makes the project profitable.

How Is the Silver Ore Extracted from the Ground?

The mining method used depends on the deposit’s shape and location. Because silver is often found in vein-type deposits, most silver-bearing mines are underground operations. This requires digging vertical shafts and horizontal tunnels, or “drifts,” to access the ore. Underground mining is more expensive and complex than surface mining. A major challenge is minimizing mining dilution. This is when non-valuable waste rock gets mixed with high-grade ore during blasting and extraction. Dilution lowers the overall metal grade sent to the processing plant, which reduces revenue. Therefore, precise drilling and blasting are essential.

Silver Mining and Exploration
Silver Mining and Exploration

Why Must You Crush and Grind Ore into Fine Powder?

This stage is called comminution. The goal of this stage is liberation. Large rocks from the mine are crushed and ground into fine particles. The material is ground until the individual mineral crystals are physically separated from the surrounding non-valuable rock (gangue). This is a required step for the silver beneficiation process. The equipment typically includes a Jaw Crusher for primary crushing, followed by a Cone Crusher. The final grinding is done in large, rotating Ball Mills. Achieving the correct particle size is important. If particles are too coarse, liberation is incomplete and silver is lost. If particles are too fine, excess energy is consumed.

Jaw Crusher
Jaw Crusher
Cone Crusher
Cone Crusher
Silver-Processing-Ball-Mill
Ball Mill

How Does Flotation Separate Silver Minerals?

For sulfide ores, froth flotation is the main separation technique. This process uses chemistry to make the silver-bearing minerals float. The finely ground ore slurry is pumped into a series of Flotation Machines. Inside these machines, chemical reagents are added that attach only to the sulfide mineral surfaces, making them water-repellent (hydrophobic). Air is then bubbled through the slurry. The hydrophobic mineral particles attach to the air bubbles and float to the surface, forming a mineral-rich froth. This froth, which contains the silver, is then collected. Because silver is often with both lead and zinc, a method called “differential flotation” is used to create separate lead-silver and zinc concentrates.

Silver ore beneficiation - flotation
Silver ore beneficiation – flotation

What Is the Alternative Path Using Cyanidation?

If the silver is in an oxidized ore and associated with gold, a different chemical process called cyanide leaching is used. This is common in a Gold CIL Plant. The finely ground ore is mixed with a weak sodium cyanide solution in large, agitated tanks. The cyanide dissolves the silver and gold, transferring them from the solid rock into the liquid solution. Pellets of activated carbon are also added to these tanks. The dissolved silver and gold adsorb onto the carbon’s surface. This “loaded” carbon is then screened out of the slurry, and the precious metals are stripped off in a separate circuit. The final product from this process is a Doré bar, a semi-pure alloy of gold and silver.

Silver cyanide
Silver cyanide
Cyanide
Cyanide

From Froth to Powder: Creating a Saleable Concentrate

The froth from the flotation cells is approximately 90% water. This water must be removed before transport. The dewatering process begins when the froth is sent to a thickener. In a thickener, gravity causes the solid particles to settle, forming a denser slurry. This slurry is then pumped to a filter press, which removes most of the remaining water. The final product is a damp powder called a “concentrate.” This concentrate is the final product that the mine sells. The mine does not produce pure silver.

How Do You Finally Get 99.9% Pure Silver Ingots?

The silver concentrate is sold and shipped to a specialized facility called a smelter. At the smelter, the concentrate is heated in a furnace to high temperatures. This process melts the metals and allows them to separate from impurities, which form a waste product called slag. This step produces impure metal bullion that contains the silver. This bullion then undergoes a final refining process, such as electrolytic refining. This last step separates the pure silver from the lead and any other remaining metals. The result is 99.9% pure silver bullion, which is cast into ingots for the market.

What Happens to the Mine After the Silver is Gone?

The operational cycle of a mine does not end when the final ore is extracted. Modern mining includes a detailed plan for mine closure and reclamation. The objective is to return the site to a safe and environmentally stable condition. This involves dismantling the processing plant and all other infrastructure. The waste rock dumps and tailings storage facilities are covered with soil and re-vegetated with native plants to control erosion. Water management systems are implemented to ensure long-term water quality. This final stage is a regulatory requirement.

About ZONEDING

Since 2004, ZONEDING has been a manufacturer of mineral processing equipment. We understand the silver mining process is a complex metallurgical procedure that requires correct technology. Our work includes more than manufacturing individual machines. We design and deliver complete, integrated silver processing solutions, from Crushing Equipment to flotation circuits. We specialize in creating custom flowsheets that match the specific mineralogy of your ore to maximize metal recovery and project revenue.

The prev: The next:

Related recommendations

We use cookies to ensure that we give you the best experience on our website. If you continue to use this site we will assume that you are happy with it.
Privacy Policy

OK
1
Scan the code